Mon-Sun: 8:00 AM - 7:00 PM J.P. Nagar 8th Phase, Bangalore
+91 95133 93125 +91 93333 38855 16+ Years of Experience
Grouting

PU Injection Grouting: Procedure and Applications

03 Sep 2026 · 4 min read · By Sai Namanaa Build Care

How polyurethane injection stops active leaks in cracks and joints, where it is used, the step-by-step procedure and what to expect.

PU injection grouting is a repair method that seals a leak from inside the crack or joint where the water is travelling. Instead of coating the surface and hoping the water stays behind it, a liquid polyurethane (PU) resin is pumped into the leak path. There it reacts, expands and forms a seal. It is one of the most useful methods for leaks that are active, under pressure or impossible to reach from the water side.

This article explains where PU injection is used, how it works, how the procedure is carried out and what its limits are.

Where PU injection grouting is used

  • Basement walls and floors with active seepage
  • Construction joints and cold joints in concrete
  • Cracks in retaining walls, sumps and water tanks
  • Leaks around pipe and cable penetrations
  • Lift pits, tunnels and podium slabs
  • Leaks that came back after surface coatings

Why surface coatings often fail on active leaks

When water is flowing or pushing through a crack, a coating applied on the face of the wall has nothing to hold on to. Water pressure lifts it, and the leak simply moves to the edge of the coating. Injection works because it stops the water inside the structure, at the crack itself.

How the resin works

Many PU injection resins react with water. When they meet the water in a wet crack, they foam or gel and fill the opening. Different resin types behave differently:

Resin typeBehaviourTypical use
Hydrophobic PUReacts quickly, foams, forms a flexible sealFast, active leaks and gushing cracks
Hydrophilic PUAbsorbs water, forms a gel that stays flexibleCracks and joints that stay damp, movement areas
Epoxy injection resinRigid, bonds concreteDry structural cracks, not active leaks

The right resin depends on whether the crack is wet or dry, how much water is flowing and whether the crack moves. This is decided after inspecting the crack, not before.

The procedure, step by step

  1. Locate and mark the leak. The crack or joint is traced along its full length and injection points are marked along it, usually on both sides in an alternating pattern.
  2. Drill the injection holes. Holes are drilled at an angle so that they cross the crack inside the concrete, at a depth that suits the member thickness.
  3. Clean the holes. Dust and debris are flushed out so that resin can flow freely.
  4. Fix the packers. Injection packers are fixed in the holes and tightened. The surface crack may be temporarily sealed so that resin does not escape at the face.
  5. Inject the resin. Resin is pumped in through the packers one at a time, starting from the lowest, until it appears at the next packer and the water flow stops.
  6. Remove packers and finish. Once the resin has cured, packers are removed, holes are filled with non-shrink grout and the surface is finished or coated.
  7. Observe and re-inject if needed. The area is watched through the next rain. If minor seepage remains, a second round of injection seals it.

Things to know before choosing PU injection

  • Injection stops the leak path. It does not replace waterproofing of the wider structure, such as a failed roof membrane.
  • Large movement joints may need a flexible sealant or joint system in addition to resin.
  • Dry structural cracks usually call for epoxy, not PU.
  • Re-injection may be needed if the structure continues to move.
  • Potable water tanks need resins whose data sheet states suitability for contact with drinking water.

Frequently asked questions

Can PU injection stop a leak that is flowing right now?

Yes. This is one of its main uses. The resin reacts with the water and expands to seal the path, although very heavy flow may need an accelerated resin or more than one round of injection.

Will it damage the concrete?

The holes are small and are filled after injection. Drilling is planned so that reinforcement is avoided as far as possible.

Do I still need waterproofing after injection?

Often a protective coating or membrane follows, especially in basements and tanks. Injection seals the crack, and the coating protects the surrounding surface.

How long does the seal last?

It depends on the resin, the movement in the structure and the conditions. We explain what to expect for your particular crack after inspecting it, and we do not promise a fixed number of years.

Next step

PU injection works best when combined with proper surface repair and a protective coating where required. See our PU injection grouting service and basement waterproofing pages, or send us photos of the leak and we will advise.

Keep reading

More technical articles

Call Engineer WhatsApp Quote